Hot deformation behavior in Al-2.35Mg alloy

Haoyan Diao,Re Han Qayyume,Tingting Wang,Shasha Zhao,Chaoli Ma
2011-01-01
Abstract:This article describes the deformation response and microstructure evolution of Al-2.35Mg alloy under uniaxial tensile testing at different temperatures (ranging from 400°C to 525°C) and strain rates (10 -2 s -1, 10 -3 s -1 & 10 -4 s -1). Under optimum deformation conditions, the said material exhibits more than 215% elongation before failure. The tensile deformation is discussed in the light of the competing influences of temperature and strain rate. The microstructures have been analyzed by optical (OM) and scanning electron microscopy (SEM). It is observed that continuous re-crystallization occurs during hot deformation of the alloy which causes reasonable enhancement of the plasticity of the coarse-grained material. Grain growth is due to high temperature and plastic deformation. The fractograph of the alloy samples after hot deformation is also analyzed. The results reveal that the fracture, on a microscopic scale, is predominantly ductile comprising microvoid nucleation, growth and coalescence.
What problem does this paper attempt to address?