Abstract:Dry sliding wear tests at 25-400 degrees C were performed for 45, 4Cr5MoSiV1 and 3Cr13 steels; the relations between oxidative wear and Cr content of steels were explored. The low and medium-Cr steels had a substantially lower wear rate and increasing tendency than the high-Cr steel at 25-200 degrees C, but the contrary case occurred at 400 degrees C. With an increase of ambient temperature, the wear rate of the low and medium-Cr steels first decreased, then increased and reached the lowest value at 200 degrees C, while the wear rate of the high-Cr steel decreased monotonously with the lowest value at 400 degrees C. At 25 degrees C, trace tribo-oxides reduced wear to some extent in adhesive-dominated wear for the low and medium-Cr steels. At 200 degrees C, a small amount of tribo-oxides formed and reached a thickness of 10 mu m on contacting asperities in the low and medium-Cr steels, thus oxidative mild wear prevailed. At 400 degrees C, a great amount of tribo-oxides appeared in the low and medium-Cr steels; unexpectedly, the high-Cr steel had more tribo-oxides than the low or medium-Cr steels in some cases. Its high wear resistance may be attributed to Cr-strengthened adhesion power of tribo-oxides and matrix. (C) 2011 Elsevier B.V. All rights reserved.
What problem does this paper attempt to address?