Transport Properties of Fe0.92mn0.08six Semiconductor Prepared by Rapid Solidification and Hot Pressing

YF Lu,XB Zhao,HL Ni,HY Chen,ZT Wu
DOI: https://doi.org/10.3321/j.issn:1002-185x.2004.09.020
2004-01-01
Rare Metal Materials and Engineering
Abstract:P-type Fe0.92Mn0.08Six(x=1.9, 2.0, 2.1, 2.3, 2.5) alloys were prepared by rapid solidification and hot pressing. XRD analysis revealed that for all samples the phases were converted into a single beta phase after being annealed for 24 h at 800 degreesC. The density of all the samples is over 90%. The experimental results showed that Fe0.92Mn0.08Si2.1 had the highest power factor over the whole measured temperature range greater than 400 muW(.)m(-1.)K(-1) at 550degreesC.