Microstructure and Strength of TiAl/40Cr Joint Diffusion Bonded with Vanadium-Copper Filler Metal

P He,JC Feng,YY Qian,BG Zhang
DOI: https://doi.org/10.3969/j.issn.1004-5341.2002.02.012
2002-01-01
Abstract:Intermetallics TiAl was diffusion-bonded to steel 40Cr in vacuum furnace with interlayer V/Cu. The results show that infinite sosoloid that made for bond performance is formed at the interface of V/Cu and Cu/40Cr, and three acting layers are formed at the interface of TiAl/V including Ti3Al layer at TiAl side, intermittent V5Al8 layer in the middle and Ti-V sosoloid at V side. Fragile reactors V5Al8 arising at the interface lead to bad performance of joints, and the strength of the joint is 200MPa, while it was still higher than the strength of the joint intermetallics TiAl to 40Cr steel diffusion-bonded directly. Intermetallic TiAl and 40Cr steel are diffusion-bonded successfully by using a composite isolation layer V/Cu.