Interface Structures and Phase Growth of TiAl/40Cr Diffusion Bonded Joint

冯吉才,李卓然,何鹏,张秉刚
DOI: https://doi.org/10.3321/j.issn:1004-0609.2003.01.030
2003-01-01
The Chinese Journal of Nonferrous Metals
Abstract:TiAl intermetallic compound was joined to 40Cr steel by diffusion bonding at the temperature range of 1 173~ 1 373 K for 0.3~5 .4 ks in vacuum. Reaction phases and interface structures were investigated by S EM, EPMA analysis and XRD diffraction method. At the bonding temperature of 1 3 73 K, four phases of TiC, Ti 3Al, FeAl and FeAl 2 were established and three layers were formed in the TiAl/40Cr joint, the interface structures were observe d as TiAl/ Ti 3Al+FeAl+FeAl 2/TiC/decarbonized layer/40Cr steel. The total rea ction layer grows with the joining time following the parabolic law, the activat ion energy Q and rate constants k 0 for the growth are 211.9 kJ/mol an d 4.6×10 -5 m 2/s respectively. At the 0.3 μm reaction layer thicknes s of TiC+Ti 3Al+FeAl+FeAl 2, the maximum strength of the TiAl/40Cr joint is up to 183 MPa at room temperature.
What problem does this paper attempt to address?