Gas-discharging Reactions in Gelcasting of Si-containing Materials and Their Effect on Microstructure of Green Bodies

ZHOU Long-jie,XU Xing-li,HUANG Yong,XIE Zhi-peng,DAI Jian-qing
DOI: https://doi.org/10.3969/j.issn.1001-4381.2000.07.009
2000-01-01
Abstract:In situ consolidation colloidal forming processes, such as gelcasting, are promising techniques for complex shapes of materials with high density, high uniformity and, thus, high reliability of performance. Si-containing powders, e.g. Si, SiC and Si3N4, are suitable for being well dispersed in alkaline solutions. However, silicon powder and free silicon contained in silicon carbide and silicon nitride powders have a tendency to hydrolyze, especially in a basic aqueous solution for gelcasting, causing a large amount of macropores in green bodies as a consequence of hydrogen gas evolution. Moreover, silicon nitride itself is chemically unstable in aqueous solutions and easy to react with other reagents when processed by aqueous gelcasting, which also affects the microstructure of green bodies. After identifying the causes of macropores formation in the gelcast green bodies, some solutions are proposed to overcome these problems.
What problem does this paper attempt to address?