On the mechanism of zircaloy-4 fatigue-deformation under different heat-treatment conditions

Lin Xiao,HaiCheng Gu
1996-01-01
Abstract:The tensional and low-cycle fatigue testing data of zircaloy-4 treated under different heat-treatment conditions were measured at room temperature and 400��C respectively, and whose fatigue deformation modes were determined by means of transmission electron microscope. The results show that (1) the zircaloy-4 under stress-relieved condition has the better combination of tensile strength and ductility than the one under recrystallization condition, but has lower fatigue lifetime; (2) {1010} prismatic slip is the primary deformation mode for zircaloy-4, whereas the pyramidal slip is activated at higher temperature and greater cyclic strain ranges; (3) at room temperature, the typical deformation structure is the parallel dislocation lines; (4) at 400��C, the square cells are formed for the stress-relieved specimens, whereas the elongated cells and the perpendicular plusdipole cells are formed for the recrystallized specimens. In addition, the fatigue mechanism was also discussed.
What problem does this paper attempt to address?