Constructing the Nanointerpenetrating Structure of PCDTBT:PC70BM Bulk Heterojunction Solar Cells Induced by Aggregation of PC70BM Via Mixed-Solvent Vapor Annealing

Jiangang Liu,Liang Chen,Bingrong Gao,Xinxiu Cao,Yanchun Han,Zhiyuan Xie,Lixiang Wang
DOI: https://doi.org/10.1039/c3ta10629b
IF: 11.9
2013-01-01
Journal of Materials Chemistry A
Abstract:In this paper, mixed-solvent vapor annealing (M-SVA) was proposed to improve polymer crystallinity and inhibit fullerene intercalation into polymer side chains in a poly[N-90-heptadecanyl-2,7-carbazole-alt-5,5- (4',7'-di-2-thienyl-2',1',3'-benzothiadiazole)] (PCDTBT):[6,6]-phenyl-C-71-butyric acid methyl ester (PC70BM) blend system. Experiments showed the optimal volume ratio of a mixed solvent, i.e., for tetrahydrofuran (THF) and carbon disulfide (CS2) vapor it is 1 : 1, and the appropriate annealing time is 5 min. After the M-SVA process, out-of-plane grazing incidence X-ray diffraction (GIXD) and spectroscopic ellipsometry (SE) data show that PCDTBT crystals with larger size and higher crystallinity were formed due to enhanced pi-pi interaction of polymer chains; the aggregation of PC70BM was promoted as well, which inhibited the intercalation behavior, resulting in a continuous electron path and improved phase purity. The morphology transition improved the carrier mobility, in particular electron mobility. Also, the recombination of a charge transfer (CT) state was reduced and the lifetime of mobile carriers was increased, which could be verified by transient-absorption (TA) spectra. As a result, the power conversion efficiency (PCE) of the BHJ reached 6.60%, an increase of more than 40% compared with the reference device (PCE = 4.54%), even though the thickness of the active layer is up to 220 nm and the PC70BM content is as low as 71.4 wt% by weight.
What problem does this paper attempt to address?