Hydrogen Absorption/desorption Behaviors over a Quaternary Mg–Ca–Li–N–H System

Yongfeng Liu,Zhitao Xiong,Jianjiang Hu,Guotao Wu,Ping Chen,Kenji Murata,Ko Sakata
DOI: https://doi.org/10.1016/j.jpowsour.2006.04.006
IF: 9.2
2006-01-01
Journal of Power Sources
Abstract:Hydrogen storage in a quaternary Mg–Ca–Li–N–H system has been investigated by XRD, FT-IR, TPD and PCI. Results showed that hydrogen desorption occurred at temperature about 50°C, and peaked at ∼178°C under a heating rate of 2°Cmin−1. The reversibility of hydrogen storage was observed and the maximum hydrogen storage capacity of about 2.7wt.% was reached at 220°C and 75atm. However, the plateau pressure for hydrogen desorption is relatively low (∼0.3atm). Structural identifications reveal that a new phase with tetragonal structure positioned at 31.8° and 51.3° of XRD peaks was generated during hydrogen absorption/desorption.