Composition and Morphology of CuInSe2 Thin Films by Electrodeposition

ZHANG Zhi-an,LIU Fang-yang,L(U) Ying,LAI Yan-qing,LI Jie,LIU Ye-xiang
DOI: https://doi.org/10.3321/j.issn:1004-0609.2007.04.010
2007-01-01
Abstract:CuInSe2 thin films were obtained by electrodeposition,and the preparation conditions and their effect on performance of CuInSe2 films were investigated.The results show that the optimum ranges of potentials for electrodeposition and annealing temperature are about -0.6--0.8 V(vs SCE) and 440-610 ℃,respectively.Annealing is a necessary step for getting high-quality CuInSe2 thin films.CuInSe2 thin films can be prepared at different deposition potentials and electrolyte concentrations.As the potential moves to negative,the concentration of CuInSe2 increases,crystallinity and uniformity become better,and impurity phase decreases.The crystallinity and density improve,and the grains grow bulkier as the concentration of electrolyte increases.In all electrodeposited CuInSe2 thin films,the potential and electrolyte concentration can influence the mole ratio of Cu to In greatly.At the potentials of-0.7 and -0.8 V(vs SCE),the mole ratio of Cu to In is very reasonable at about 1.The change of mole ratio of Cu to In has the same trend as that of CuCl2 to InCl3 in electrolyte.
What problem does this paper attempt to address?