M23C6 Precipitation in 00Cr25Ni35AITi by Aging Treatment

Zhi-peng GUO,Zhi-gang SONG,Wen-jie ZHENG,Han FENG,Wen CHEN
2009-01-01
Abstract:The precipitation behavior of M23C6 in 00Cr25Ni35AlTi after aging treatment at 550-950 ℃ has been studied.The results show that M23C6 mainly precipitates at grain boundary and the end of twin and M23C6 is in the coherency with the matrix while there is no evidence of M23C6 existed in the coherent twin boundary and matrix.The content and size of M23C6 precipitation increase with the aging temperature from 550 to 850 ℃.The morphology of M23C6 also turns from thin rods into flake,then acute triangular form in the end.The content of M23C6 decreases as the result of dissolution at temperature ranging from 850 to 950 ℃.