Microstructure and properties of Ti-Cr alloys used for dentistry

XU Li-juan
2010-01-01
The Chinese Journal of Nonferrous Metals
Abstract:Ti-Cr alloys were fabricated by using tungsten electrode melting and centrifugal casting.Microstructure and mechanical properties of Ti-Cr alloys were investigated.The dry wear resistance of Ti-Cr alloys against Gr15 ball was investigated on CJS111A ball-disk wear instrument.The influence of alloy element Cr on alloys wear resistance was investigated.Worn surface morphologies were observed by scanning electron microscope(SEM).The maximum wear scar depth of Ti-Cr alloys was measured by electron microprobe analyzer.The wear mechanism of Ti-Cr alloys was analyzed.The results show that crystal structure and morphology of the cast Ti-Cr alloys are sensitive to their chromium contents.The Vickers hardness of the Ti-Cr alloy decreases with the increase of the chromium concentration.The highest compression strength of Ti-10Cr alloy is 2 024 MPa and the lowest compression strength of Ti-15Cr alloy is 1 650 MPa. Ti-5Cr alloy shows a smallest steady friction coefficient and the worn surface is comparatively smooth.For Ti-15Cr and Ti-20Cr alloys,the phenomenon of furrow cut happens and furrows form during wear tests.Wear tests show that the increasing Cr content leads to a reduction of wear depth of Ti-Cr alloys and increase of wear resistance.The wear mechanism for Ti-Cr alloys is a combination of adherence wearing and debris wearing.
What problem does this paper attempt to address?