Synthesis and Characterization of Samaria Stabilized Zirconia Powders by Buffer-Solution Method

Cheng Jigui,Shi Ping,Li Jie,Dong Jie,Xia Yonghong,Meng Guangyao
DOI: https://doi.org/10.3321/j.issn:1000-4343.2007.01.006
2007-01-01
Abstract:Zirconia stabilized with 4%~12%(mole fraction) samaria(4~12 SSZ) powders were synthesized by a buffer-solution method.Phase constitute,particle size and morphology of the synthesized powders was characterized by X-ray diffraction (XRD),transmission electron microscopy(TEM) and BET,respectively.The powders were cold isostatic pressed and sintered at 1300~1500 ℃ for 5 h.Density of the sintered SSZ samples was measured by the Archimedes method and were expressed as relative to the theoretical value,and microstructure was observed by scanning electron microscope(SEM).Electrical conductivity and conductive activation energy of the sintered SSZ samples were also tested in the temperature range 500~800 ℃ in air by alternating-current impedance spectroscopy.The results show that SSZ powders with single fluorite phase can be obtained by calcining the coprecipitates at a relatively low temperature of 600 ℃.The powders have regular particle shape with an average particle size of 10~20 nm.The samaria amount and the calcination temperature also have a great influence on the phase formation.Density of the sintered SSZ samples increases as sintering temperature and Sm2O3 doping amount increase.A relative density of 96.91% is obtained for the 12 SSZ sample sintered at 1500 ℃.Electrical conductivity of the sintered SSZ samples increases with temperature.The 12 SSZ sample sintered at 1500 ℃ has an ionic conductivity of 0.043 S·cm-1 and a conductive activation energy of 0.72 eV at 800 ℃ in air.
What problem does this paper attempt to address?