Hard Magnetic Properties of Sm3fe26.7vxn4 and Sm3fe26.7vxcy

XF Han,MC Zhang,Y Qiao,FM Yang,CP Yang,GC Liu,YZ Wang,BP Hu
DOI: https://doi.org/10.1016/s0304-8853(98)00538-1
IF: 3.097
1999-01-01
Journal of Magnetism and Magnetic Materials
Abstract:Sm3Fe26.7V2.3N4 nitrides and Sm3Fe26.7V2.3Cy carbides have been synthesized by gas–solid phase reaction. Their hard magnetic properties have been investigated by means of additional ball-milling at room temperature. The saturation magnetization of Sm3Fe26.7V2.3N4 almost decreases linearly with increasing ball-milling time t, but that of Sm3Fe26.7V2.3Cy has no obvious change when the ball-milling time increases from t=1 to 28h. As a preliminary result, the maximum remanence Br of 0.94 and 0.88T, the coercivity μ0iHC of 0.75 and 0.25T, and the maximum energy product (BH) of 108.5 and 39.1kJ/m3 for their resin-bonded permanent magnets are achieved, respectively, by ball-milling at 293K.
What problem does this paper attempt to address?