Fracture process zone of autoclaved aerated concrete

MA Chang-chen,FENG Nai-qian
DOI: https://doi.org/10.3969/j.issn.1002-3550.2008.11.002
2008-01-01
Abstract:The complete curves of load-the opening displacements at several points along initial crack and its ligament are determined by using three point bend beams of autoclaved aerated concrete with different initial relative crack lengths.The results show that there exists a linear distribution of crack opening displacements along initial crack and its ligament under the descending part of load—the opening displacement complete curves,and at the same time the average crack opening angle and the crack mouth opening displacement have a linear relation,which is independent of initial relative lengths.While load level(P/Pmax)is constant,the length of fracture process zone is bigger if the initial crack relative length is smaller.