Residual Life Assessment of X20CrMoV12.1 Straight Main Steam Pipe in Service

HU Zheng-fei,YANG Zhen-guo
DOI: https://doi.org/10.3969/j.issn.1672-4763.2007.03.005
2007-01-01
Abstract:The main steam pipe in a thermal power plant in Shanghai degraded obviously after 23 years in service.Its mechanical properties displays embrittlement tendency,and correspondin microstructure exhibits granule boundary weakening and creep damage characteristics,however no creep cavitation or surface crack was found.The results of stress rupture strength tests and stress analysis show that it is possible to obtain a life of greater than 100,000 hours of this straight steam pipe under normal service condition.It is recommended that a health assessment should be taken after 50,000 hours sevice exposure for safety.
What problem does this paper attempt to address?