Research on Preparation and Characterization of Forsterite(Mg2SiO4)by Solid State Reaction

孙成礼,张树人,周晓华,李波
2008-01-01
Abstract:Mg_2SiO_4 is prepared from Mg(OH)_2·4MgCO_3·6H_2O and SiO_2 by the solid state reaction sinter route.The results show that the single-phase Mg_2SiO_4 powder can be obtained when the mixtures with Mg:Si ratio of 2:1.2 is presintered at above 1200℃for 3h in air.The samples sintered at 1280~1340℃for 2h show a low tanδin the range of(2~5)×10~(-4) withe_r of 7.05±0.05 measured at 1MHz.The bulk density of obtained ceramic is(3.1±0.5) g/cm~3.