Spark Plasma Sintering and Mechanical Properties of ZrO2(Y2O3)–Al2O3 Composites

JS Hong,L Gao,SDDL Torre,H Miyamoto,K Miyamoto
DOI: https://doi.org/10.1016/s0167-577x(99)00225-6
IF: 3
2000-01-01
Materials Letters
Abstract:Spark plasma sintering (SPS) was conducted on nanocrystalline ZrO2(Y2O3)–20 mol% Al2O3 powder at a heat rate of 600°C/min with a short holding time. Full density was obtained at sintering temperatures >1300°C. Considerable grain growth occurred relative to the initial powder particles, but smaller grain size and higher density can be obtained as compared to hot-pressing. High flexural strength and fracture toughness were also achieved for the SPS-resulted composite.