Ba6-3xNd8+2xTi18O54 MICROWAVE DIELECTRIC CERAMICS PREPARED BY THE HYDROTHERMAL METHOD

WANG Hui,XU Jianmei,SU Yanjie,GONG Wenqiang
DOI: https://doi.org/10.3321/j.issn:0454-5648.2007.02.005
2007-01-01
Abstract:Ternary Ba6-3xNd8+2xTi18O54 ceramics were prepared by the hydrothermal method.The phase compositions of the ceramics were characterized by X-ray diffraction and the properties of the ceramics were also measured.The results show that using Nd(OH)3 or TiCl4 as a precursor,pure phase Ba6-3xNd8+2xTi18O54 ceramics powders can be prepared by the hydrothermal method at 360 ℃ for 12 h,and the synthesis temperature of ceramics powders can be reduced.The sintering temperature for synthesizing Ba6-3xNd8+2xTi18O54 ceramic powders is 1 250 ℃,about 100 ℃ lower than that of the conditional solid-state method.The ceramic material has a little higher dielectric constant,better temperature coefficient of resonance frequency and quality factor.When x=2/3,the Ba6-3xNd8+2xTi18O54 ceramic has the best microwave dielectric properties,with a dielectric constant of 88,a product of quality factor and resonance frequency of 8 890 GHz,and a temperature coefficient of frequency of 24×10-6/℃.
What problem does this paper attempt to address?