NORMAL SINTERING OF LEAD-FREE PIEZOCERAMIC POTASSIUM SODIUM NIOBATE AND ITS ELECTRICAL PROPERTIES

ZHANG Limin,ZHANG Boping,LI Jingfeng,WANG Ke,ZHANG Hailong
DOI: https://doi.org/10.3321/j.issn:0454-5648.2007.01.001
2007-01-01
Abstract:Potassium sodium niobate ceramic with a nominal composition of Na0.5K0.5NbO3 (NKN) was fabricated successfully by sintering at 1 020—1 100 ℃ and normal pressure. The effect of sintering temperature on the density, structure and the electric proper- ties of NKN ceramics were investigated. The results show that the crystal phase of the NKN ceramics is an orthorhombic structure similar to that of KNbO3 ceramics, a second phase formed when the sintering temperature is higher than 1 080 ℃. The density of the sintered NKN ceramics changed dramatically in a narrow temperature range of 1 020—1 100 ℃. The density of the ceramics sintered at 1 080 ℃ reached a maximum value of 4.22 g/cm3 (92% of the theoretical density). The ceramic sintered at 1 060 ℃ shows a maximum piezoelectric coefficient of about 122 pC/N and a maximum Curie temperature of 409 ℃, and the coercive field and rema- nent polarization are 9 kV/cm and 15 μC/cm2, respectively.
What problem does this paper attempt to address?