Microwave Properties of Bst and Bst/Bmt Thin Films Grown on Sapphire Substrate by Evanescent Microwave Probe

PT Joseph,YC Chen,YH Chu,HF Cheng,NH Tai,IN Lin
DOI: https://doi.org/10.1080/10584580500414044
2005-01-01
Integrated Ferroelectrics
Abstract:Thin films of BaxSr1-xTiO3 (BST) serial materials have the advantages of adjustable tunability and are good candidates for the application in DRAM and microwave devices. However, these films usually have loss tangent higher than the order of 0.01 at microwave frequencies. To improve the crystal structures and suppress the microwave losses, an interlayer material with good microwave properties can be used. In this present work, a low loss Ba(Mg1/3Ta2/3)O-3 (BMT) thin buffer layer with varying thickness and its effect on the microwave properties of Ba0.4Sr0.6TiO3 thin films is investigated. Moreover, to overcome the spatial limit in the traditional microwave measurement, a novel technique, evanescent microwave probe (EMP) method, is used to directly probe the microwave dielectric properties of the films. This technique also provides the capability to study the dielectric mechanism in micro-scale region.Pulsed laser deposition technique was used to synthesize thin films. The films shows (111) preferably oriented growth of BST films with the introduction of BMT layer for the films grown on sapphire substrates. As the thickness of BMT increases, this behavior is more obvious. The microwave dielectric constants (epsilon) and dielectric losses (tan delta) of the films grown on sapphire substrates have been measured by EMP. The dielectric constants of BST thin films decrease monotonously with the increase of BMT thickness. In contrast, the tan delta shows a discontinuity variation when the BMT buffer layer is deposited for 10-20 minutes.
What problem does this paper attempt to address?