The study on preparation and thermal stability of nanocrystalline LaF3 bulk material

Wu Daxiong,Wu Xijun,Lu Yanfei,Wang Hui
2006-01-01
Rare Metal Materials and Engineering
Abstract:Nanocrystalline powder of LaF3 With an average grain size of 16.7 nm was synthesized by a method of direct precipitation from water solution. Nano-LaF3 bulk material was prepared by compacting the powder to 1 GPa at room temperature and a vacuum of 10(-4) Pa. The grain size of the nano-LaF3 bulk material annealed at various temperatures was measured by X-ray diffraction. The results indicated a grain size increase from 16.7 nm to 92.6 nm when the annealing temperature rose to 900 degrees C. The DSC curves of nano-LaF3 bulk material were measured at heating rates of 5 K / min, 10 K / min, 1 5 K / min and 20 K / min, respectively. According to the Kissinger equation, the activation energy for grain growth of nano-LaF3 bulk material was calculated to be 2.01 eV or 233 kJ / mol.