Effect of severe plastic deformation realized by rotary swaging on the mechanical properties and corrosion resistance of near-a-titanium alloy Ti-2.5Al-2.6Zr

V. N. Chuvil'deev,V. I. Kopylov,A. V. Nokhrin,P. V. Tryaev,N. Yu. Tabachkova,M. K. Chegurov,N. A. Kozlova,A. S. Mikhaylov,A. V. Ershova,M. Yu. Grayznov,I. S. Shadrina,C. V. Likhnitskii
DOI: https://doi.org/10.1016/j.jallcom.2019.01.268
2024-01-31
Abstract:The research aims to analyze the impact that severe plastic deformation arising during Rotary Swaging has on mechanical properties and corrosion resistance of a near-a-titanium alloy Ti-2.5Al-2.6Zr (Russian industrial name PT7M). The nature of corrosion decay in fine-grained alloys caused by hot salt corrosion is known to vary from pit corrosion to intercrystalline corrosion at the onset of recrystallization processes. Resistance to hot salt corrosion in a fine-grained titanium alloy Ti-2.5Al-2.6Zr is shown to depend on the structural-phase state of grain boundaries that varies during their migration as a result of covering corrosive doping elements (aluminum, zirconium) distributed in the crystal lattice of a titanium alloy.
Materials Science
What problem does this paper attempt to address?
The paper aims to study the effects of severe plastic deformation induced by Rotary Swaging on the mechanical properties and corrosion resistance of near-α titanium alloy Ti-2.5Al-2.6Zr (Russian industrial name PT7M). Specifically: 1. **Mechanical Properties**: Through rotary swaging treatment, a fine-grained structure is formed, significantly improving the material's yield strength, ultimate strength, and hardness. However, this also leads to a decrease in the material's ductility. 2. **Corrosion Resistance**: The study found that in the coarse-grained state, the alloy exhibits two types of corrosion defects in high-temperature salt corrosion tests: one related to β-phase particles and the other related to intergranular corrosion (ICC) associated with corrosive dopant elements (such as zirconium and aluminum) distributed along the grain boundaries. In the fine-grained state, the corrosion behavior changes over time, gradually transitioning from pitting corrosion to intergranular corrosion. This transition may be related to the migration of grain boundaries during recrystallization, leading to an increased concentration of corrosive dopant elements at the grain boundaries. In summary, the main objective of the paper is to improve the mechanical properties and corrosion resistance of near-α titanium alloy Ti-2.5Al-2.6Zr through the rotary swaging process and to explore the specific effects of microstructural changes on these properties.