Fabrication of high performance silicon nitride ceramics with TiO2 additive by annealing process

Yusen Duan,Jingxian Zhang,Boan Zhou,Xiaoguang Li,Qun Wang,Ning Liu,Zhe Li,Lingfeng Wang
DOI: https://doi.org/10.1016/j.ceramint.2022.11.059
IF: 5.532
2023-03-01
Ceramics International
Abstract:The high performance Si3N4 ceramic was prepared firstly for TiO2, Y2O3 and MgO as pressureless sintering additives. Si3N4 ceramic with relative density of 99.6% and flexural strength of 785 ± 23.3 MPa could be obtained with 3 mol% TiO2 and sintered at 1800 °C for 2 h. After annealing at 1700 °C, the facture toughness of sample of 1 mol% TiO2 increased from 8.31 ± 0.28 MPa m1/2 to 9.84 ± 0.16 MPa m1/2. The flexural strength of sample of 2 mol% TiO2 increased from 707 ± 26 MPa to 981 ± 16 MPa, thermal conductivity increased from 57.8 W/(m·K) to 68.49 W/(m·K). The XRD results showed that the ratio of I 101/I 210 and grain height reached to 1.84 and 5 μm of the sample of 3 mol% TiO2, respectively. The present investigation revealed that the three-dimensional array of highly oriented crystalline Si3N4 micro rods could be prepared which array on the homogeneous substrates by using TiO2 as agent. This phenomenon may propose a method that the mechanical properties the Si3N4 ceramics added TiO2 can be improved significantly after annealing process.
materials science, ceramics
What problem does this paper attempt to address?