Method for producing medium and low carbon aluminum killed steel

曾建华,杨森祥,陈小龙,陈天明,李桂军,陈亮,李清春,雷辉,陈永
2011-06-30
Abstract:The invention provides a method for producing medium and low carbon aluminum killed steel, which comprises the following steps of: controlling the content of sulfur in molten iron to be not more than 0.015 percent; primarily smelting the molten iron to form molten steel, and tapping; adding an aluminum deoxidizer into the molten steel when 20 to 30 weight percent of molten steel is tapped; adding4.0 to 6.0kg of active lime and fluorite in an amount which is 0.2 times that of the active lime into each ton of molten steel when 31 to 50 weight percent of molten steel is tapped; performing argonblowing refining for the first time; adding aluminum in two or three batches and 1.5 to 4kg of refining slag into each ton of steel in a steel ladle, heating, and refining; performing calcium treatment on the molten steel; performing argon blowing refining for the second time; and performing continuous casting. By the method, the castability of the molten steel can be improved, the phenomenon of water nozzle clogging is avoided, and the continuous casting heats of a single tundish in the continuous casting process of the medium and low carbon aluminum killed steel are not less than 8 heats.
Materials Science
What problem does this paper attempt to address?