Weak antilocalization and gigahertz acoustic phonons in Bi2Se2Te and Bi3Se2Te-dominated thin films grown using pulsed laser deposition

Phuoc Huu Le,Le Thi Cam Tuyen,Nguyen Nhat Quyen,Chih-Wei Luo,Jiunn-Yuan Lin,Jihperng Leu
DOI: https://doi.org/10.1016/j.tsf.2024.140241
IF: 2.1
2024-02-01
Thin Solid Films
Abstract:We reported a comparative study on the material–magnetotransport properties of topological insulator Bi2Se2Te and a ternary Bi3Se2Te-dominated thin films. The Bi-Se-Te thin films were grown on c-plane sapphire using pulsed laser deposition at various substrate temperatures (TS ) of 180 – 300 °C. The highly c-axis-oriented films exhibited the Bi2Se2Te phase (at TS = 180, 220 °C), and a mixed phase of dominant Bi3Se2Te and mimor Bi2Se2Te (at TS = 260, 300 °C). In addition, XPS and EDS results confirmed the near stoichiometry compositions of Bi2Se2Te and Bi3Se2Te phases. In high magnetic fields, the magnetoresistance (MR) curves of Bi2Se2Te and Bi3Se2Te obeyed B2 power law, and the carrier mobility was determined to be increased monotonically from 61.3 to 86.9 cm2/Vs when TS increased from 180 to 300 °C. In low magnetic fields, MR curves of both Bi2Se2Te and Bi3Se2Te-dominated films presented two-dimensional weak antilocalization at low temperatures, possibly due to topological surface states in the thin films. Furthermore, we observed two acoustic phonon modes at 33.46 ± 0.69 GHz and 61.30 ± 1.75 GHz in both Bi2Se2Te and Bi3Se2Te-dominated thin films induced by ultrafast laser pulses.
materials science, multidisciplinary,physics, applied, condensed matter, coatings & films
What problem does this paper attempt to address?