Fabrication and bending behavior of amorphous SiC-fiber-reinforced Si-Co eutectic alloy composites at elevated temperatures

Toru Tsunoura,Katsumi Yoshida,Toyohiko Yano,Takuya Aoki,Toshio Ogasawara
DOI: https://doi.org/10.1016/j.compositesb.2019.01.103
2019-05-01
Abstract:Amorphous SiC-fiber-reinforced Si-CoSi2 and CoSi2–CoSi eutectic alloys composites have been developed by a melt infiltration method, and their mechanical properties were evaluated at elevated temperatures up to 1220 °C. As compared to polycrystalline Si, Si–Co ingots showed a ductile transition at a lower temperature (200–400 °C) due to the ductile transition of CoSi2 and the presence of a debonding interface. Moreover, the composites using Si–Co alloys showed superior bending behavior at elevated temperatures around 1000 °C as compared to composites using Si because of the ductile behavior of the Si–Co alloys and the prevention of the degradation of the SiC fibers.
What problem does this paper attempt to address?