Amalgam Protection for Alkali Metal Anodes
Guang He,Qingwen Li,Qi Zhang,Yi Ding
DOI: https://doi.org/10.1149/ma2020-01191mtgabs
2020-01-01
ECS Meeting Abstracts
Abstract:The dendrite issue and the associated cell degradation problems have proved to be a key challenge to the practical application of alkali metal anodes.1,2 We present a simple yet efficient approach to fabricate amalgam anodes (Figure 1a) that afford long-term stability cycling at practical current densities and capacities.3 The amalgam layer allows fast electron transfer as well as Li/Na/K migration at the electrolyte-electrode interphase, which significantly promote the cycling performance. For example, Protected Li electrodes exhibit stable cycling over 750 hrs at high plating current and capacity of 8 mA cm-2 and 8 mAh cm-2 in symmetric cells (Figure 1b). Coupled with high-loading cathodes (~12 mg cm-2) such as LiFePO4 (LFP) and LiNi0.6Co0.2Mn0.2O2 (NCM), the prototype full cells also demonstrate much improved rate and long-term cycling stability (Figure 1c). In-situ optical microscopy analyses confirm the dendrite nucleation and growth can be remarkably suppressed with the Li-Hg protected anodes (Figure 1d). These promising results provide new perspectives on the regulation of sodium electrodeposition and hence the elimination of the dendritic morphology for the practical development of alkali metal batteries. References: 1. X.-B. Cheng, R. Zhang, C.-Z. Zhao, and Q. Zhang, Chem. Rev., 117, 10403–10473 (2017). 2. R. Weber, M. Genovese, A. J. Louli, S. Hames, C. Martin, I. G. Hill, and J. R. Dahn, Nat. Energy, 4, 683-689 (2019). 3. G. He, Q. Li, Y. Shen, and Y. Ding, Angew. Chem. Int. Ed., DOI: 10.1002/anie.201911800 (2019). Figure 1. a) The preparation process of Li-Hg protected anodes; b) Cycling performance of Li-Hg protected anodes and pristine anodes in symmetric cells; c) Cycling performance of Li-Hg protected anodes and pristine anodes in full cells with high-loading LFP and NCM cathodes; d) In-situ optical analyses showing the different Li deposition behaviors on Li-Hg protected and pristine anodes. Figure 1