Fatigue endurance limit and crack front evolution in metallic glass

Xianqi Lei,Lichao Yuan,Liu Peng,Chengqi Sun,Bingchen Wei,Yujie Wei
DOI: https://doi.org/10.1016/j.ijfatigue.2020.106004
IF: 5.489
2021-02-01
International Journal of Fatigue
Abstract:<p>Fatigue endurance limit is a threshold stress-amplitude under which a solid subjected to a cyclic loading can sustain infinite life. Such a limit has been confirmed in ferrous materials but remains controversial in many advanced new materials, including bulk metallic glasses with superb strength. By using a combination of ultrasonic fatigue (USF) test and conventional fatigue test, we obtain the stress amplitude vs. loading cycle curve of the Vitreloy 1<sup>TM</sup> metallic glass, with loading cycles up to <span class="math"><math>109</math></span>. There is a clear fatigue endurance limit (FEL) which is about 320 MPa, and is 17% of the strength of Vitreloy 1<sup>TM</sup>. The residual strength of survivals after 10<sup>9</sup> cycles is nearly the same as those of intact samples. We demonstrate that all fatigue cracks initiate from spherical pores which are inevitable and intrinsic amid casting and fast cooling, and the fatigue crack front resembles an ellipse arc till final rapid rapture of all tested samples. The size and position of a pore can be utilized to extract the fatigue initiation threshold <span class="math"><math>K0th</math></span>, and the elliptical fatigue crack front is used to obtain the mode I fracture toughness <span class="math"><math>KIC</math></span>, which are <span class="math"><math>K0th=2.0±0.5MPam</math></span> and <span class="math"><math>KIC=1820MPam</math></span> for Vitreloy 1<sup>TM</sup>, respectively. The fatigue endurance limit and its intrinsic origin of Vitreloy 1<sup>TM</sup> pave the way to understand fatigue in other metallic glasses.</p>
materials science, multidisciplinary,engineering, mechanical
What problem does this paper attempt to address?