Reconfiguring Organosulfur Cathode by Over-Lithiation to Enable Ultrathick Lithium Metal Anode toward Practical Lithium–Sulfur Batteries

Zhipeng Jiang,Hui-Juan Guo,Ziqi Zeng,Zhilong Han,Wei Hu,Rui Wen,Jia Xie
DOI: https://doi.org/10.1021/acsnano.0c06133
IF: 17.1
2020-09-14
ACS Nano
Abstract:An ultrathick lithium metal anode (LMA) is a prerequisite for developing practical lithium–sulfur (Li–S) batteries that simultaneously meet the requirements of high areal capacity, lean electrolyte, and limited excess Li. Inspired by the electrochemical process for an organosulfur cathode, herein, we reconfigure such a sulfur cathode by using an overlithiation strategy to enable the formation of a high performance LMA. Specifically, an applicable ultrathick LMA is successfully constructed by overlithiating a well-known organosulfur cathode material, sulfurized polyacrylonitrile (SPAN). SPAN contains a polymeric pyridine structure with an outstanding lithium-ion affinity, so that it can act as a lithiophilic matrix. More importantly, a Li<sub>2</sub>S-rich solid electrolyte interphase (SEI) can be generated on the surface of SPAN during the overlithiation process. The synergistic effect of the lithiophilic matrix and a robust SEI leads to a dense deposition of lithium, which enables one to form an ultrathick LMA (159 μm, 30 mAh cm<sup>–2</sup>) with high Coulombic efficiency (99.7%). Such an LMA paired with a sulfur cathode of high areal capacity (up to 16 mAh cm<sup>–2</sup>) shows stable cycling under practical conditions of a lean electrolyte (2.2 μL mg<sub>S</sub><sup>–1</sup>) and a negative-to-positive capacity (N/P) ratio as low as 1.3. The applicability of the ultrathick LMA was further verified with Li–S pouch cells, indicating a highly prospective route toward realization of practical Li–S batteries.The Supporting Information is available free of charge at <a class="ext-link" href="/doi/10.1021/acsnano.0c06133?goto=supporting-info">https://pubs.acs.org/doi/10.1021/acsnano.0c06133</a>.Figures S1–S17, structural characterizations of SPAN; SEM images of pristine ; initial Li plating/stripping curve of ; EIS plots for the Li–Li symmetric cells; charge/discharge curves of ∥S full cell; schematic illustration of the cell for <i>in situ</i> optical microscopy; XRD pattern of ; XPS S 2p spectra of Cu-LMA; normalized TOF-SIMS depth profiles; cross-profile images of TOF-SIMS depth sputtering; SEM images of ultrathick cathode; SEM images of the cycled ; ultrathick Se<sub>0.05</sub>S<sub>0.95</sub>PAN cathode paired with Li foil in different electrolyte; Tables S1 and S2, elemental analysis result of different samples and estimated Li–S batteries energy densities (<a class="ext-link" href="/doi/suppl/10.1021/acsnano.0c06133/suppl_file/nn0c06133_si_001.pdf">PDF</a>)This article has not yet been cited by other publications.
materials science, multidisciplinary,chemistry, physical,nanoscience & nanotechnology
What problem does this paper attempt to address?