Atmospheric Leaching Behavior and Kinetics Study of Roasted Laterite Ore

Gyan Prameswara,Idi Amin,Andi Nurfaadhilah Ulfah,Iga Trisnawati,Himawan Tri Bayu Murti Petrus,Fitria Puspita
DOI: https://doi.org/10.1007/s42461-024-00947-x
2024-02-27
Abstract:Laterite ore is a valuable resource due to its high content of metals essential for modern technology, including nickel, iron, and cobalt. However, extracting nickel from laterite ores is challenging due to their complex mineral composition and low nickel concentrations. This study examined the leaching behavior of pre-roasted laterite ore and the effect of roasting on leaching kinetics. The ore was roasted at temperatures of 280°C and 610°C for 3 h, followed by sulfuric acid atmospheric leaching. The results demonstrated that pre-roasting at 610°C significantly enhanced nickel leaching recovery, with up to 93% nickel successfully recovered. The leaching process of pre-roasted laterite ore was found to be controlled by diffusion through the ash layer, with activation energy values of 20.97 and 18.97 kJ/mol for laterite roasted at 280°C and 610°C, respectively. These findings indicate that pre-roasting can improve the leaching performance of laterite ore, potentially leading to more efficient and sustainable nickel extraction processes.
mining & mineral processing,metallurgy & metallurgical engineering
What problem does this paper attempt to address?