Degradation of LaPO 4 -8YSZ composite thick thermal barrier coatings by molten calcium-magnesium-aluminosilicate

Wenzhi Huang,Ruiqi Zhong,Xin Zhou,Panhao Deng
DOI: https://doi.org/10.1016/j.jeurceramsoc.2024.116863
IF: 5.7
2024-08-26
Journal of the European Ceramic Society
Abstract:The effect of LaPO 4 content on the calcium-magnesium-aluminosilicates (CMAS) corrosion resistance of the plasma-sprayed LaPO 4 -8YSZ composite coatings at 1250 °C was investigated. The microstructure and corrosion products of the LaPO 4 -8YSZ composite coatings after CMAS attack was determined by using SEM/TEM/SAED. The results indicated that LaPO 4 was segregated at the grain boundaries of the composite coatings and the addition of LaPO 4 into 8YSZ coating increased their CMAS reactivity, which led to the formation of planar reaction zone while the CMAS infiltration depth decreased from ~658 μm to ~119 μm. The CMAS infiltration depth of the composite coatings firstly increased with LaPO 4 addition, reaching its maximum for the composite coating with 5 wt.% LaPO 4 , and then showed a downtrend. For the composite coating with 20 wt.% LaPO 4 , a dense apatite layer formed in the corrosion front, which inhibited CMAS penetration and resulted in the shallowest CMAS infiltration depth among the test samples.
materials science, ceramics
What problem does this paper attempt to address?