The significant impact of grain refiner on -TiAl intermetallic fabricated by laser-based additive manufacturing
Danni Huang,Qiyang Tan,Yinghao Zhou,Yu Yin,Feng Wang,Tao Wu,Xianliang Yang,Zhiqi Fan,Yingang Liu,Jingqi Zhang,Han Huang,Ming Yan,Ming-Xing Zhang
DOI: https://doi.org/10.1016/j.addma.2021.102172
IF: 11
2021-01-01
Additive Manufacturing
Abstract:Intermetallic gamma-TiAl alloy has been considered as a promising structural material for high temperature use, owing to their advantages such as low density, high creep strength and good toughness. However, due to its intrinsic brittleness, gamma-TiAl alloy could not accommodate the high thermal stress generated by fast cooling during laserbased additive manufacturing (LAM) process, resulting in cracking and distortion. To surmount the roadblock of low processability associated with gamma-TiAl alloy, grain refinement technology was integrated to LAM. In the present work, LaB6 nanoparticles were identified and experimentally verified, for the first time, as an effective inoculant for LAMed gamma-TiAl alloy. The results showed that the grain size of the as-printed alloy drastically decreased from 39.81 +/- 9.12 mu m to 1.5 +/- 2.07 mu m through 0.5 wt% LaB6 addition. Accordingly, the microstructural morphology transformed from coarse near-lamellar colonies into equiaxed and fine grains. The LaB6 inoculation treatment not only led to the fabrication of crack-free alloy but concurrently increases in compressive yield strength, ultimate strength and strain to fracture by 29%, 12.4% and 61.9%, respectively. Such an enhanced performance is comparable with or even better than the gamma-TiAl alloys produced using conventional processing techniques.