Effect of surface Nd-rich phase and oxygen content of melt-spun flakes on formation of coarse grains in hot-pressed Nd-Fe-B magnet

Yeyuan Du,Wenzong Yin,Renjie Chen,Xu Tang,Jinyun Ju,Bin Chen,Longquan Hou,Aru Yan,Jianhui Yuan
DOI: https://doi.org/10.1016/j.jre.2020.09.018
IF: 4.632
2021-11-01
Journal of Rare Earths
Abstract:Nd-Fe-B hot-pressed (HP) magnet prepared from melt-spun MQU-F flakes features coarse grains (CG) with the average size of both 200 nm (CG<sub>S</sub>) and 700 nm (CG<sub>L</sub>) at flake boundary. The grain growth at the flake boundary of Nd<sub>2</sub>Fe<sub>14</sub>B/α-Fe composite HP magnet before and after diffusion of low-melting-point Pr<sub>82</sub>Cu<sub>18</sub> phase was investigated, revealing the indispensable role of surface RE-rich phase of melt-spun flakes in the formation of CG in HP magnet. The dominant role of surface oxygen content of melt-spun flakes in the formation of CG<sub>L</sub> has been clarified with etching method. The HP magnet prepared from the etched flakes with dramatically decreased oxygen content exhibits the CG regions merely with homogeneous equiaxed CG<sub>S</sub> at flake boundary. Consequently, the coercivity (<em>μ</em><sub>0</sub><em>H</em><sub>c</sub>) shows significant increase while remanent magnetization (<em>μ</em><sub>0</sub><em>M</em><sub>r</sub>) inappreciable change. Further investigation with sieving method revealed the elimination of CG<sub>L</sub> via removal of the fine Nd-Fe-B flakes smaller than 54 μm due to their much higher oxygen content, confirming the dominant role of oxygen content in the formation of CG<sub>L</sub>. The quantitative analysis on the magnetic properties of the above HP magnets revealed the monotonic increase of coercivity (<em>μ</em><sub>0</sub><em>H</em><sub>c</sub>) and negligible change of remanent magnetization (<em>μ</em><sub>0</sub><em>M</em><sub>r</sub>) with decreased oxygen contents of Nd-Fe-B flakes. The maximum value of coercivity (<em>μ</em><sub>0</sub><em>H</em><sub>c</sub>) has increased from 2.26 T to 2.47 T as the oxygen content decreased from 0.1692 wt% to 0.079 wt%.Coarse grains (CG) regions of the hot-pressed magnets prepared from etched Nd-Fe-B flakes (a) and sieved Nd-Fe-B flakes (b) (&gt;54 μm) exhibit equiaxed CG with homogeneous size (c, d) and morphology near flake boundary (FB), rather than the coexistence of small CG (average size of 200 nm) and large CG (average size of 700 nm).<span class="display"><span><ol class="links-for-figure"><li><a class="anchor download-link u-font-sans" href="https://ars.els-cdn.com/content/image/1-s2.0-S1002072120304117-fx1_lrg.jpg"><span class="anchor-text">Download : <span class="download-link-title">Download high-res image (317KB)</span></span></a></li><li><a class="anchor download-link u-font-sans" href="https://ars.els-cdn.com/content/image/1-s2.0-S1002072120304117-fx1.jpg"><span class="anchor-text">Download : <span class="download-link-title">Download full-size image</span></span></a></li></ol></span></span>
chemistry, applied
What problem does this paper attempt to address?