High-Temperature Storage Deterioration Mechanism of Cylindrical 21700-Type Batteries Using Ni-Rich Cathodes under Different SOCs

Daozhong Hu,Qiyu Zhang,Jun Tian,Lai Chen,Ning Li,Yuefeng Su,Liying Bao,Yun Lu,Duanyun Cao,Kang Yan,Shi Chen,Feng Wu
DOI: https://doi.org/10.1021/acsami.0c20835
2021-01-28
Abstract:The safety and energy density of lithium-ion batteries (LIBs) are important concerns. The use of high-capacity cathode materials, such as Ni-rich cathodes, can greatly improve the energy density of LIBs, but it also brings some safety hazards. Cylindrical 21700-type batteries using Ni-rich cathodes were employed here to investigate their high-temperature storage deterioration mechanism under different states of charge (SOCs). Electrolyte decomposition was identified as the main problem. It can be worsened by elevated storage temperatures and battery SOCs, with the latter having a more significant influence. Specifically, the decomposition of the LiPF<sub>6</sub> solute and the carbonate solvent will induce hydrofluoric acid (HF) formation and solid–electrolyte interphase (SEI) film regeneration, respectively. HF erosion will aggravate the dissolution of transition metal ions and structural degradation of cathode materials, while the destruction/regeneration of SEI films will consume active lithium and hinder Li<sup>+</sup> diffusion at the anode side. Besides, the self-discharge behavior will also enlarge the graphite layer spacing, thus decreasing the graphitization degree of graphite anodes and causing anode failure. These findings will aid in the development of strategies for improving the safety of LIBs with high energy density.The Supporting Information is available free of charge at <a class="ext-link" href="/doi/10.1021/acsami.0c20835?goto=supporting-info">https://pubs.acs.org/doi/10.1021/acsami.0c20835</a>.Nyquist plots of all of the batteries stored at different temperatures and battery SOCs. SEM images of the stored cathode and anode electrodes with EDS elemental mappings at different temperatures and battery SOCs. The fitted result of XPS Ni 2p spectra for cathodes stored at different temperatures and battery SOCs. TEM images of the stored cathodes in batteries under 75 °C-100% SOC. XRD patterns of the stored cathode and anode materials at different temperatures and battery SOCs. SEM images and the EDS result for element species on both sides of the separator. Element content of the cathode material in 21700-type batteries calculated from ICP-OMS. The quantitative results of all of the XPS spectra in <a class="internalNav" href="#fig3">Figures </a><a class="internalNav" href="#fig3">3</a>, <a class="internalNav" href="#fig4">4</a>,<a class="internalNav" href="#fig10">10</a>, and <a class="internalNav" href="#fig11">11</a> (<a class="ext-link" href="/doi/suppl/10.1021/acsami.0c20835/suppl_file/am0c20835_si_001.pdf">PDF</a>)This article has not yet been cited by other publications.
materials science, multidisciplinary,nanoscience & nanotechnology
What problem does this paper attempt to address?
The paper aims to study the degradation mechanisms of 21700 cylindrical cells with high-nickel cathode materials under high-temperature storage conditions at different states of charge (SOC). Specifically, the paper explores the following aspects: 1. **Electrolyte Decomposition**: The study found that electrolyte decomposition is the main cause of battery performance degradation. As temperature and SOC increase, lithium hexafluorophosphate (LiPF6) in the electrolyte decomposes to produce hydrofluoric acid (HF), which then corrodes the cathode material, leading to the dissolution of transition metal ions and structural phase changes. Additionally, the decomposition of carbonate solvents can cause the regeneration of the solid electrolyte interface (SEI) film, consuming active lithium and hindering lithium-ion diffusion on the anode side. 2. **Impact of SOC on Battery Performance**: Compared to the impact of temperature, SOC has a more significant effect on battery performance. High SOC leads to more severe capacity loss and increased internal resistance. Particularly under high SOC conditions, the surface of the cathode undergoes a transition from a layered structure to a rock-salt structure, further obstructing lithium-ion transport and exacerbating capacity decay. 3. **Self-Discharge Behavior**: High-temperature storage accelerates the self-discharge process, increasing the interlayer spacing of graphite, reducing the degree of graphitization, and ultimately leading to anode failure. 4. **Separator Changes**: High-temperature storage also causes the separator to melt and pores to clog, affecting lithium-ion transport and increasing polarization. Through these studies, the paper provides theoretical basis and technical guidance for improving the safety of high-energy-density lithium batteries.