Surface Modification Improves Spinel LiCoO2 Li-Ion Battery Cathode Materials Grown by Low Temperature Solvothermal Flow Reaction

Yan Zhang,Umair Gulzar,Alex Lonergan,Alex Grant,Aoife Carroll,Ahin Roy,Valeria Nicolosi,Tony Keene,Colm O'Dwyer
DOI: https://doi.org/10.1149/1945-7111/ad1e41
IF: 3.9
2024-01-13
Journal of The Electrochemical Society
Abstract:Methods that provide routes to LiCoO2 growth with lower energy requirements from recycling battery cathode ashes are important for sustainable Li-ion battery technology growth. Here, a low temperature route to a stable, coated spinel-phase LT-LCO material with secondary Co3O4 phase can be achieved at 300°C directly from the layered double hydroxide [Li2(ox)2][Co5(OH)8] product of solvothermally synthesized LiOH and CoCl2. The low-temperature LiCoO2 materials (known as LT-LCO) consist of spinel-phase LCO and secondary Co3O4 phase. When used as cathode in lithium batteries, we used a solution-based method of coating with an ionic conductor LiAlO2 with AlF3 to mitigate sluggish reversible lithiation kinetics and the poor cycling and rate performance of as-synthesized spinel LT-LCO. The coating modification promotes reversible lithium ion transfer and stabilizes the spinel structure. The modified LT-LCO cathode has significantly better overall capacity and rate performance, with a capacity retention of ~80 mAh g-1 after 150 cycles (factoring the LT-LCO and Co3O4 mass). The initial first cycle coulombic efficiency significantly improves to >95%. The data show that even spinel phase LCO grown by this solvothermal route cycles stably with a useful specific capacity and rate response in the voltage range of 2.0 to 4.2 V.
electrochemistry,materials science, coatings & films
What problem does this paper attempt to address?