Experimental Investigations into the Effect of Infill Patterns on the Microstructure and Mechanical Properties of Inconel 718 Using Laser-Directed Energy Deposition

Varsharani Gaikhe,Anish Ranjan,Shrikrishna N. Joshi
DOI: https://doi.org/10.1007/s11665-024-10311-1
IF: 2.3
2024-11-01
Journal of Materials Engineering and Performance
Abstract:Inconel 718 is a demanding superalloy in aerospace, energy, marine and oil and gas industries due to its exceptional strength, creep behaviour and corrosion resistance in extreme temperature spectrum. In recent years metal additive manufacturing (MAM) of Inconel 718 has drawn significant attention due to its good weldability and poor machinability. However, numerous process parameters of MAM techniques, such as laser type, energy density, scanning speed, scanning strategies, infill pattern, layer thickness, form of feedstock and feed rate, frequently impact the structure and performance of IN718 components. This paper presents experimental investigations into the Laser Directed Energy Deposition (LDED) of Inconel 718. Four infill patterns, namely wiggle, rectilinear, honeycomb, and triangular, were employed to print rectangular cuboidal samples of Inconel 718 wire using LDED. The infill pattern governs the heat input, heat distribution, and cooling rates which significantly controls the microstructure evolution and ultimately affects the mechanical properties of the parts. The effect of infill patterns on the microstructure and mechanical properties of coupon samples were thoroughly investigated. Microstructure and mechanical properties at room temperature were found distinct for different infill strategies. The samples printed with the triangular pattern provide poor aesthetics but the highest yield strength (540 MPa) and hardness (261–276 HV) owing to the large concentration of small-sized grains and precipitation of the secondary phases. However, samples printed using a rectilinear infill pattern contain large-sized columnar grains, resulting in the highest elongation (35%) with the lowest yield strength (465 MPa) and hardness (240-258 HV). The honeycomb patterns offer superior aesthetics along with moderate strength and hardness compared to the rectilinear and triangular patterns.
materials science, multidisciplinary
What problem does this paper attempt to address?