Improvement of the Bonding Strength of A2/Cu Interface by Co, Ni, P and B Addition in Planar Flow Casting Process Based on First-principle Calculations

Rui Guo,Siqian Bao,Yifei Feng,Deming Xu,Yuanyao Cheng
DOI: https://doi.org/10.1016/j.mtcomm.2023.106899
IF: 3.8
2023-08-17
Materials Today Communications
Abstract:Introduction of alloying elements into interface is proven effective in improving bonding strength of the A2/Cu interface, which improves surface quality of silicon steel strip in the planar flow casting (PFC) process. In this research, we explored how the additions of Co, Ni, P and B influence interfacial bonding by the first-principles method. The method does not rely on other empirical parameters, and only needs five basic physical constants. Starting from the chemical composition and crystal structure of the material, various ground state properties of the material can be obtained by solving the Schrodinger equation. Five various interfaces were constructed due to different stacking sequences and interface IV has the highest work of adhesion (W ad ), 3.24 J/m 2 . Co and Ni dopants can enhance W ad and improve interfacial bonding, but P and B dopants cannot. When doping amounts increase, W ad value of Co and Ni doped interfaces continuously rises from 0 J/m 2 to 176.52 J/m 2 and 351.05 J/m 2 , respectively. The larger W ad value represents a stronger interfacial bonding. 3.5 wt% doping amounts for Co (3.24 at%) and Ni (3.25 at%) were demonstrated appropriate to strengthen interfacial bonding when the influences of doped atoms on magnetic properties of A2 phase are considered. Electronic structure is also analyzed, and the results suggest bonds in interface models are the mix of covalent and metallic bonds, and Co and Ni addition can strengthen the interfacial bonding. Therefore, the dope of 3.5 wt% Co or 3.5 wt% Ni content into silicon steel was considered optimal to strengthen interfacial bonding, and further improve the surface quality of the strip and reduce strip adhesion phenomenon during preparation process. These results also can provide a theoretical guide for fabricating high-quality silicon steel strip in PFC process.
materials science, multidisciplinary
What problem does this paper attempt to address?