Flexural strength and hardness of short-silk fiber-reinforced composite with silane addition

Dyah A Widyasrini,Mutiara Annisa,Siti Sunarintyas,Harsini Harsini
DOI: https://doi.org/10.4103/jioh.jioh_63_23
2023-01-01
Journal of International Oral Health
Abstract:Abstract Aim: To investigate the optimum concentration of silane added in fiber-reinforced composites (FRCs) and its effect on flexural strength and surface hardness. Methods and Material: The degumming process was conducted by soaking the chopped Bombyx mori silkworm cocoons in Na 2 CO 3 solution, hydrolyzing them with NaOH, and neutralizing them with hydrochloric acid. Then, lyophilization and ultra-sonification were carried out. Bombyx mori short-silk fibers (±1.49 μm) were placed into a silane solution with concentrations of 0%, 0.5%, 1%, and 1.5%. After silanation, fibers were mixed in a composite resin matrix. The volume fraction of the fiber used was 10%. Flexural strength and surface hardness tests employed 48 samples in beam and disc shapes, respectively. Each group included six samples. Flexural strength was tested using a universal testing machine and surface hardness using a microhardness tester in accordance with ISO 4049 (2000). Data obtained were analyzed statistically by analysis of variance (ANOVA), followed by a post hoc least significant difference test. Results: In the ANOVA test, a significant difference was found in the flexural strength and surface hardness among the four FRC groups ( P < 0.05). In the post hoc test, the flexural strength of the FRC group with 0.5% silane was significantly different from other groups ( P < 0.05). Meanwhile, the surface hardness of samples added with 0.5% silane was not significantly different from those added with 1% and 1.5% silane ( P < 0.05). Conclusions: Thus, 0.5% silane might be the optimal concentration to obtain FRCs with appropriate flexural strength and surface hardness.
What problem does this paper attempt to address?