Carbon-Fiber-Reinforced Epoxy Resin with Sustainable Additives from Silk and Rice Husks for Improved Mode-I and Mode-II Interlaminar Fracture Toughness

Cuong Manh Vu,Quang-Vu Bach,Huong Thi Vu,Dinh Duc Nguyen,Bui Xuan Kien,Soon Woong Chang
DOI: https://doi.org/10.1007/s13233-020-8010-7
IF: 2.127
2019-08-09
Macromolecular Research
Abstract:<p class="a-plus-plus">This paper presents an effective method for enhancing both the mode I (<em class="a-plus-plus">G</em><sub class="a-plus-plus"><em class="a-plus-plus">IC</em></sub>) and mode II (<em class="a-plus-plus">G</em><sub class="a-plus-plus"><em class="a-plus-plus">IIC</em></sub>) interlaminar fracture toughness of carbon fiber reinforced epoxy resin (CFRE). For precursor materials, silk fibroin nanofibers (nSF) and rice husk silica were prepared from sustainable resources. Nanocomposite samples were prepared using various loading ratios of the silica and nSF in epoxy resin (EP). Mechanical stirring and sonication techniques were used to prepare homogenous mixtures of silica and nSF in epoxy resin. Non-isothermal differential scanning calorimetry and the Kissinger equation were used to examine and calculate the cure kinetics and activation energy (<em class="a-plus-plus">E</em><sub class="a-plus-plus"><em class="a-plus-plus">a</em></sub>) of EP and the composite samples. The CFRE sample with hybrid fillers of nSF and silica at the ratio 0.2/20 (wt%/wt%) exhibited the highest <em class="a-plus-plus">G</em><sub class="a-plus-plus"><em class="a-plus-plus">IC</em></sub>, and improved upon the mode-I and mode-II toughness of the pure-resin sample by 36.08% and 30.06%, respectively. Study of the fracture surfaces indicated that adding nSF and silica as fillers increases the energy required to fracture the CFRE.</p>
polymer science
What problem does this paper attempt to address?