Wear and corrosion behaviour of the cryogenically treated tungsten carbide coatings

Akshay R. Govande,B. Ratna Sunil,Ravikumar Dumpala
DOI: https://doi.org/10.1080/02670844.2023.2218204
IF: 2.451
2023-06-07
Surface Engineering
Abstract:The WC–12Co coatings were deposited on SS 410 substrates using a high-velocity oxygen fuel (HVOF) process and the coatings were heat-treated at 750°C for 1 h in argon environment. Further, the coatings were subjected to cryogenic treatment for 1, 2, 8 and 24 h, and its influence on the reciprocating sliding wear and corrosion characteristics was studied. The structural changes in the coatings after post-treatment were assessed by X-ray diffraction analysis and Raman spectroscopy. Microhardness was improved for cryogenically treated coatings due to the α-Co transformation into ε-Co. Cryogenic treatment duration was not having a significant effect on the microhardness values. However, the specific wear rate was influenced by the cryogenic treatment duration. Also, corrosion resistance was increased with the increased cryogenic treatment duration. The protective layers consisting of WO 3 and Co 3 O 4 phases formed during the cryogenic treatment are attributed to the improved corrosion resistance of the coatings.
materials science, coatings & films
What problem does this paper attempt to address?