Chemical degradation of magnesium potassium phosphate cement pastes during leaching by demineralized water: Experimental investigation and modeling

Laura Diaz Caselles,Céline Cau Dit Coumes,Pascal Antonucci,Angélique Rousselet,Adel Mesbah,Valérie Montouillout
DOI: https://doi.org/10.1016/j.cemconres.2024.107456
IF: 11.958
2024-02-09
Cement and Concrete Research
Abstract:The long-term durability of magnesium potassium phosphate cement (MKPC) pastes was investigated by examining their leaching behavior. MKPC comprised magnesium oxide (MgO) and potassium dihydrogen phosphate (KH 2 PO 4 ) in equimolar amounts and yielded K-struvite (MgKPO 4 ·6H 2 O) and a nearly neutral pore solution pH upon hydration. Semi-dynamic leaching tests were performed on MKPC paste samples using demineralized water with a pH set at 7, and the leached solids were analyzed using XRD, SEM/EDS, 11 B and 31 P MAS-NMR spectroscopy. Leaching was mainly governed by diffusion of dissolved species through the pore network of the paste. Three main zones were observed in the leached solids: ( i ) a poorly cohesive residual layer where K-struvite was fully depleted, ( ii ) an intermediate zone where K-struvite coexisted with cattiite (Mg 3 (PO 4 ) 2 ·22H 2 O), and ( iii ) a third zone without any cattiite. Reactive transport modeling made it possible to predict the extent of degradation and the phase evolution in the MKPC paste samples.
construction & building technology,materials science, multidisciplinary
What problem does this paper attempt to address?