DEVELOPMENT OF THE COMBINED TECHNOLOGICAL PROCESS OF BLANK STACKS FLANGES FORMATION BY THE METHOD OF STAMPING BY ROLLING AND ROTARY DRAWING

Viktor Matviychuk,Mykola Kolisnyk
DOI: https://doi.org/10.37128/2306-8744-2021-1-11
2021-03-23
Vibrations in engineering and technology
Abstract:The article presents the results of the development and research of the combined technological process of forming the outer and inner flanges of the lids of fractional and distillation columns on sheet blanks by the method of stamping by rolling and rotary drawing. For this purpose, equipment has been developed that allows to form both outer and inner flanges of the blank in one run of the conical roll. Studies have shown that technological capabilities of the process are limited by the risk of destruction of the top layers of the outer flange bending center and its corrugation, as well as by the neck formation or destruction of the peripheral areas of the inner flange. To assess the deformability of the outer flange, the stress-strain state of its bending center was investigated. According to the set stress values, the stress state of the material is determined, the maximum value of which on the surface of the bending zone is Formula for determining the minimum radius of the mandrel, which when using the values of the critical ductility of the material allows to prevent destruction. As well, an expression for determining the maximum width of the flange, provided that the destruction of peripheral areas is prevented, is obtained. As corrugations formation is the main danger in forming the external flanges by the stamping by rolling method (SR), the expression for determining the maximum width of the flange under the condition of a stable process is obtained. If it is necessary to get more developed flanges, it is proposed to provide thinning of their walls by rotary extraction at the second stage. When forming the inner flanges of the blank stacks radial compressive stresses and tangential tensile stresses in the material are brought about. The action of tangential stresses causes loss of stability of the flange by way of neck formation. The value of the critical strains increases with the approach to the state of plain-strain deformation. Therefore, it is recommended to develop process parameters based on construction of the critical strains diagrams.
What problem does this paper attempt to address?