Effect of Exposure Temperature on Oxidation of Austenitic Steel HR3C in Supercritical Water

Zhongliang Zhu,Hong Xu,Hasan Izhar Khan,Dongfang Jiang,Naiqiang Zhang
DOI: https://doi.org/10.1007/s11085-018-9879-9
IF: 2.2
2018-11-15
Oxidation of Metals
Abstract:Oxidation tests of the austenitic steel HR3C were conducted at 600–700 °C in supercritical water under 25 MPa. The characteristics of oxide scales formed on HR3C were investigated using gravimetry, grazing incidence X-ray diffraction, electron back-scatter diffraction, scanning electron microscopy, and energy-dispersive X-ray spectroscopy. The oxidation kinetics obeyed a near-parabolic law at 600 °C but followed a near-cubic law at 620–700 °C. The oxide films consisted of an Fe-rich outer layer and a Cr-rich inner layer. The phase constitution of the outer layer was Fe2O3 and Fe3O4, while the inner layer was spinel. Moreover, a continuous Cr2O3 formed at the oxide/steel interface during exposure at 700 °C.Graphical Abstract
metallurgy & metallurgical engineering
What problem does this paper attempt to address?