Influence of Interwire Distance and Arc Length on Welding Process and Defect Formation Mechanism in Double-Wire Pulsed Narrow-Gap Gas Metal Arc Welding

Guoqiang Liu,Xinhua Tang,Siyuan Han,Haichao Cui
DOI: https://doi.org/10.1007/s11665-021-05888-w
IF: 2.3
2021-06-18
Journal of Materials Engineering and Performance
Abstract:The effects of interwire distance (<b><i>d</i></b>) and arc length correction coefficient (<b><i>C</i></b><sub><b><i>c</i></b></sub>) on the arc behaviors, droplet transfer and welding process stability in the double-wire narrow-gap gas metal arc welding (NG-GMAW) were investigated. With <b><i>d</i></b> changing from 10mm to 20mm, the arc deflection only occurs at the background stage of pulsed welding current, and the droplet transfer mode keeps unchanged. A large <b><i>C</i></b><sub><b><i>c</i></b></sub> (20%) leads to serious peak arc deflection and unstable droplet transfer, whereas a small <b><i>C</i></b><sub><b><i>c</i></b></sub> (− 10%) eliminates the arc deflection and brings about short-circuiting droplet transfer. The arc interruption frequently occurs when <b><i>d</i></b> is 20mm or <b><i>C</i></b><sub><b><i>c</i></b></sub> is 20%. Moreover, when <b><i>d</i></b> is 10mm or <b><i>C</i></b><sub><b><i>c</i></b></sub> is 20%, serious sidewall arcs occur in double-wire NG-GMAW. With the increase in <b><i>d</i></b> and/or decrease in <b><i>C</i></b><sub><b><i>c</i></b></sub>, the welding process stability can be improved at first and then gets worse. In general, the trailing arc is more stable than the leading arc. Increasing <b><i>C</i></b><sub><b><i>c</i></b></sub> will result in a serious surface depression defect on the left side of the weld bead because of the serious peak arc deflection. A sound weld bead is obtained when the interwire distance is 15mm.
materials science, multidisciplinary
What problem does this paper attempt to address?