Ferromagnetic resonance in amorphous (FeNi)80P10B10 alloys. II. Resonance near the curie temperature

L. Kraus,Z. Frait,J. Schneider
DOI: https://doi.org/10.1002/pssa.2210640205
1981-04-16
physica status solidi (a)
Abstract:Ferromagnetic resonance at room temperature is measured on amorphous (Fe1−xNix)80P10B10 very thin wires with 0.74 ≦ x ≦ 0.84. FMR measurements in the frequency range from 9.2 to 70 GHz are supplemented by static measurements of magnetization. With increasing Ni content, x, the Curie temperature decreases passing room temperature at approximately x = 0.80. Near this composition the resonance linewidth rapidly increases and its frequency dependence significantly changes. FMR data in the vicinity of Tc can be explained by a combination of two relaxation terms in the equation of motion and a g‐factor dependent on applied magnetic field. Ferromagnetische Resonanz an sehr dännen amorphen (Fe1−xNix)80P10B10‐Drähten wird für 0,74 ≦ x ≦ 0,84 bei Zimmertemperatur gemessen. Die FMR Messungen im Frequenzbereich von 9,2 bis 70 GHz werden durch statische Messungen der Magnetisierung ergänzt. Die Curie‐Temperatur fallt mit steigendem Ni‐Gehalt, sie ist nahe der Zimmertemperatur annähernd x = 0,80. In der Nahe dieser Zusammensetzung wächst die Resonanzlinienbreite sehr schnell und ihre fre‐quenzabhängigkeit ändert sich wesentlich. Die FMR‐Angaben in der Umgebung von Tc kann man mit Hilfe einer Kombination von zwei Relaxationsgliedern der Bewegungsgleichung und eines vom äußeren Magnetfeld abhängigen g‐Faktors erklären.
What problem does this paper attempt to address?