Optimisation of hybrid process to recover zinc from electric arc furnace dust using design of experiment approach

Wahidur Rahman Sajal,Sazzad Ahmad,Fahmida Gulshan
DOI: https://doi.org/10.1080/00084433.2024.2357899
2024-06-02
Canadian Metallurgical Quarterly
Abstract:Recoverable metals like zinc and iron are present in the dust from electric arc furnaces (EAF), a byproduct of the steelmaking process. These metals are mainly present as zinc ferrite (ZnFe 2 O 4 ), magnetite (Fe 3 O 4 ), and zinc oxide (ZnO) compounds. ZnO is easily dissolved in either an acidic or an alkaline solution; however, ZnFe 2 O 4 is more difficult to dissolve. Therefore, our earlier paper suggested the thermodynamic analysis of a preliminary caustic-roasting treatment to transform the ZnFe 2 O 4 from EAF dust into more soluble products of ZnO and NaFeO 2 . Finally, the present study carried out a hybrid process that involved the caustic roasting of EAF dust and a caustic leaching of the roasted product. At first, the effects of caustic-roasting process parameters on zinc-ferrite conversion were studied using the Taguchi method. The implication of Design of Experiment (DoE)-Taguchi analysis and the analysis of variance (ANOVA) shows the optimum caustic-roasting conditions are: roasting temperature of 350 o C, NaOH/ EAF dust molar ratio of 4, and roasting time of 60 minutes. The effect of temperature, reaction time, NaOH concentration, and solid/liquid (S/L) ratio was also examined using the same method in the subsequent caustic-leaching process. Similarly, the analysis shows that maximum Zn dissolution is possible at a NaOH concentration of 6M, a leaching temperature of 40 o C, a liquid-to-solid ratio of 60 ml/g, and a leaching time of 60 minutes. After the hybrid process, the zinc recovery was 83%, while most iron oxides remained in the leach residue.
metallurgy & metallurgical engineering
What problem does this paper attempt to address?