Tuning texture and precipitation using Y/Gd atomic ratio in iso-concentration Mg–Y–Gd–Ag–Zr extruded alloys

Yu Zhang,Wei Rong,Yujuan Wu,Liming Peng
DOI: https://doi.org/10.1016/j.matchar.2020.110473
IF: 4.537
2020-09-01
Materials Characterization
Abstract:<p>Three Mg-Y(Gd)-Ag-Zr alloys with an iso-concentration of total alloying elements but different Y/Gd atomic ratios were hot extruded at 350 °C and their microstructures and mechanical properties were comparatively studied. Extruded Mg-2.4Y-0.4Ag-0.1Zr (at.%) base alloy shows a bimodal-grained structure composed of fine equiaxed recrystallised grains and coarse elongated unrecrystallised grains and has a <span class="math"><math>011¯0</math></span>//ED (extrusion direction) texture. In contrast, when Y is partially replaced with Gd, extruded Mg–1.6Y-0.8Gd-0.4Ag-0.1Zr (at.%) and Mg-0.8Y-1.6Gd-0.4Ag-0.1Zr (at.%) alloys with the Y/Gd atomic ratio of 2 and 0.5, respectively, exhibit a near fully recrystallised structure and have a [0001]//ED texture. While basal γ″ precipitates dominate but few β′ precipitates form in Mg-2.4Y-0.4Ag-0.1Zr alloy, a large number density of both β′ and γ″ precipitates form in Mg-1.6Y-0.8Gd-0.4Ag-0.1Zr and Mg-0.8Y-1.6Gd-0.4Ag-0.1Zr alloys after post-extrusion ageing. Precipitation in the Gd-containing alloys is considerably enhanced by partial substituting Y with Gd. The peak-aged Mg–1.6Y–0.8Gd–0.4Ag–0.1Zr alloy keeps a relatively good balance between grain boundary strengthening, dispersion strengthening and precipitation hardening and thus obtains a good combination of strength and ductility, whose room temperature tensile yield strength, ultimate tensile strength and elongation are 377 MPa, 479 MPa and 8.0%, respectively.</p>
materials science, multidisciplinary,metallurgy & metallurgical engineering, characterization & testing
What problem does this paper attempt to address?