Oxygen-free calcination for enhanced leaching of valuable metals from spent lithium-ion batteries without a reductant

Dongxing Wang,Wei Li,Shuai Rao,Jinzhang Tao,Lijuan Duan,Kuifang Zhang,Hongyang Cao,Zhiqiang Liu
DOI: https://doi.org/10.1016/j.seppur.2020.118212
IF: 8.6
2021-03-01
Separation and Purification Technology
Abstract:<p>Drawbacks such as reductant need in leaching process or high energy consumption in pre-treatment step exist in current approaches for recycling spent lithium-ion batteries (LIBs). Here, we report an energy-saving pre-treatment process that can increase the metals leaching efficiency of spent LiNi<em><sub>x</sub></em>Co<em><sub>y</sub></em>Mn<sub>1−</sub><em><sub>x</sub></em><sub>−</sub><em><sub>y</sub></em>O<sub>2</sub> LIBs in H<sub>2</sub>SO<sub>4</sub> solution. In the proposed process, the spent electrode material was calcined in a nitrogen (oxygen-free) atmosphere, resulting in the easy leaching of metals by H<sub>2</sub>SO<sub>4</sub> without adding reductant. Calcination conditions were examined, and calcination at 350 °C for 1.5 h resulted in the optimal leaching rates of Li, Ni, Co, and Mn (&gt; 99%). Mechanism analysis revealed how calcination improves the leaching efficiency. We found the proposed calcination pre-treatment can destroy the well-defined layered crystal structure of spent LiNi<em><sub>x</sub></em>Co<em><sub>y</sub></em>Mn<sub>1−</sub><em><sub>x</sub></em><sub>−</sub><em><sub>y</sub></em>O<sub>2</sub> without changing its original phase composition. As a result, refinement of crystalline size, increase of defect, amorphization, and specific surface area (with the emergence of cracks and voids) of the cathode particles enhance the leaching of metals. This study may provide an energy-saving and cost-effective pre-treatment process that can remarkably improve metals leaching rates from spent LIBs without adding reductants.</p>
engineering, chemical
What problem does this paper attempt to address?