Strengthening Valuable Metal Recovery from Spent Lithium-Ion Batteries by Environmentally Friendly Reductive Thermal Treatment and Electrochemical Leaching

Shuya Lei,Yintao Zhang,Shaole Song,Rui Xu,Wei Sun,Shengming Xu,Yue Yang
DOI: https://doi.org/10.1021/acssuschemeng.1c00937
2021-04-21
Abstract:The traditional acid leaching method for recycling valuable metals from the cathode material of spent lithium-ion batteries (LIBs) has encountered the problems of high consumption of H<sub>2</sub>SO<sub>4</sub> and reducing agents. In this study, a novel process has been developed to strengthen valuable metal recovery from spent lithium-ion batteries by reductive thermal treatment and electrochemical leaching. With the help of reductive thermal treatment under the conditions of <i>R</i> = 1600 °C and 120 min, the layered structure of the cathode material LiNi<sub>1/3</sub>Co<sub>1/3</sub>Mn<sub>1/3</sub>O<sub>2</sub> is reduced to a mixture of Li<sub>2</sub>CO<sub>3</sub>, NiO, Co<sub>3</sub>O<sub>4</sub>, Mn<sub>2</sub>O<sub>3</sub>, and MnO<sub>2</sub> due to the oxygen releasing from the framework. The destruction of the layered crystal structure reduces the difficulty of leaching valuable metals. 90.59% Ni, 90.53% Co, 66.40% Mn, and 100% Li were leached under the optimal conditions of 20 mL/g liquid–solid ratio, 1.5 M H<sub>2</sub>SO<sub>4</sub>, 0.8 A, and 150 min at room temperature. Comparing the processes of reductive thermal treatment with acid leaching and direct electrochemical leaching of spent cathode material under the same leaching conditions, the proposed approach can achieve the highest metal recovery and economic benefits. It can be implemented at room temperature, decreases the application of reducing agent and sulfuric acid, and makes full use of spent graphite, resulting in a greener recycling process for recovering valuable metals from spent LIBs.The Supporting Information is available free of charge at <a class="ext-link" href="/doi/10.1021/acssuschemeng.1c00937?goto=supporting-info">https://pubs.acs.org/doi/10.1021/acssuschemeng.1c00937</a>.XRD pattern of spent cathode materials, the picture of roasted product under conditions of <i>R</i> = 1, at 600 °C for 180 min, XPS of Ni, Co, and Mn for the electrochemical residues under conditions of 1.5 M H<sub>2</sub>SO<sub>4</sub>, 0.8 A for 150 min, the composition of spent cathode materials, calculation of the cost, benefit, and profit, and comparison of leaching valuable metals by proposed and existing methods (<a class="ext-link" href="/doi/suppl/10.1021/acssuschemeng.1c00937/suppl_file/sc1c00937_si_001.pdf">PDF</a>)This article has not yet been cited by other publications.
chemistry, multidisciplinary,engineering, chemical,green & sustainable science & technology
What problem does this paper attempt to address?
The problem that this paper attempts to solve is the high consumption of acids and reducing agents in the traditional methods for recovering valuable metals from spent lithium - ion batteries. Specifically, the traditional acid leaching method for recovering valuable metals (such as nickel, cobalt, and manganese) from the cathode materials of spent lithium - ion batteries requires a large amount of sulfuric acid and reducing agents, which not only increases the cost but also brings the risk of environmental pollution. Therefore, the researchers have developed a new process flow by combining reductive heat treatment with electrochemical leaching, aiming to improve the recovery rate of valuable metals while reducing the usage of acids and reducing agents, and achieving a more environmentally - friendly and economic recovery process. The core of this new method lies in destroying the layered crystal structure of the cathode material through reductive heat treatment, converting it into metal oxides and lithium carbonate that are more easily leached, thereby reducing the energy and chemical consumption required in the leaching process. The experimental results show that under the optimal conditions (i.e., the reductive heat treatment conditions are 1600 °C, 120 minutes, and the electrochemical leaching conditions are a liquid - solid ratio of 20 mL/g, 1.5 M H₂SO₄, a current of 0.8 A, and a reaction time of 150 minutes), the recovery rates of nickel, cobalt, manganese, and lithium reach 90.59%, 90.53%, 66.40%, and 100% respectively, showing the significant advantages of this method in improving metal recovery rates and economic benefits.